Dow Chemical has launched a new generation of materials for the development of electric vehicles.



The development of the electric vehicle industry has always been a hot topic and a major trend for the future. Regarding the key materials needed for the development of electric vehicles, the Sil-More Group continues to pay attention to industry dynamics and provide solutions. This time, we will quickly introduce three materials launched by Dow Chemical for electric vehicles: DOWSIL™ TC-4060 GB250 thermal conductive gel, DOWSIL™ TC-2035 CV thermal conductive adhesive, and DOWSIL™ TC-4551 CV thermal conductive sealant. With high thermal conductivity, they undoubtedly provide good results in heat dissipation, excellent dielectric insulation to protect sensitive components, and control technology for low molecular siloxane volatiles, which can prevent internal components from being affected by volatiles, greatly enhancing overall reliability and stability, and assisting the development of the electric vehicle industry. They are very suitable for the power systems of hybrid electric vehicles (HEV) and electric vehicles (EV), as well as driving assistance systems (ADAS) and engine control units (ECU).

 

◆DOWSIL™ TC-4060 GB250 Thermal Conductive Gel Features:

● Ultra-high thermal conductivity (~6 W/m・K)

● Room temperature curing or heat accelerated curing

● Good stability in high temperature environments

● Low volatile content (D3-D12) <100ppm

● Provides stress relief and shock protection

● Excellent insulation strength >7.5 KV/mm

● Thickness control 250µm

● Shelf life at room temperature 12 months

Watch the DOWSIL™ TC-4060 GB250 video

 

 

 

 

 

 

◆DOWSIL™ TC-2035 CVAdhesiveFeatures:

● High thermal conductivity (3.3 W/m・K)

● Thermal curing (115°C/15 minutes)

● Good stability in high temperature environments

● Low volatile content (D4-D10) <100ppm

● Can achieve low seam thickness

● Shelf life at room temperature 12 months

Watch the DOWSIL™ TC-2035 CV video

 

 

 

 

 

 

◆DOWSIL™ TC-4551 CVThermal ConductiveSealantFeatures:

● High thermal conductivity (5.2 W/m・K)

● Room temperature curing or heat accelerated curing

● Good stability in high temperature environments

● Low volatile content (D4-D10) 13ppm

● Soft and compressible after curing

● UL 94 V-0 (0.15mm & 3.0mm)

※E-MobilityInformation related to innovative materials for electric vehicleshttps://www.silmore.com.tw/tc/emobility

※ Please subscribe to ourYouTubechannel andnewsletter, Sil-More will periodically provide new product promotions, product technology, industry information, and related videos.
※ For further assistance, please feel free to call during business hours at +886-2-85122222 orclick hereto inquire by email, and a professional sales team will contact you.
※ Data source: Dow Chemical TDS